EPX 66 is a trowelled flooring system based on a three-component epoxy, used mainly when high mechanical load is required

المواصفات

اللمسة النهائية flat (ASTM-D523)
العبوة Component A “base” : 1.7 L in metal can Component B “drier:CAT40” : 0.6 in metal can Component C “special filler” : 8 kg “diameter: 0.5 to 1 mm approx.” or 16 kg “diameter: 3 to 6 mm” (dry and dust free), or according to needs with different diameter ranges. Mixing of components A, B, and C will pro
اللون Translucent
الرمز EPX66
Application Instruction — Mixing Ratio 1.7 to 0.9 L (A to B); the required quantity of clean, dry and dust free filler or special stones (component C) will be added according to the filler or stone diameter that will fit with the flooring thickness to be applied. Pretest a small amount of filler or stones to determine the required weight
Application Instruction — Mixing The individual components (A and B) of EPX66 should be thoroughly stirred. Then component B “drier” should be poured into component A “base” container and mixed thoroughly using a slow speed mixer for at least 3 minutes to achieve uniform consistency; “DO NOT USE HIGH SPEED MIXER”. And finally add t
Application Instruction — Pot life 30 minutes (higher temperatures will shorten the potlife sharply)
Application Instruction — Thinner / Cleaner Do not thin. Due to Potlife limitations, clean all mixing and applying tools by thinner S405 “known as Epoxsol” immediately after application is completed
Technical Information — Volume Solids 100 %. (ASTM-D2697)
Technical Information — Recommended film thickness 1-4 cm “dry”
التغطية (م²/لتر) 0.1 m²/L at 1cm “dry”
Technical Information — Water resistance Good
Technical Information — Abrasian Resistance Good
Technical Information — Chemical Resistance Good (A separate leaflet CHR01 is available)
Technical Information — Solvent Resistance Good (A separate leaflet CHR01 is available)
عدد الطبقات 1
Technical Information — Specific Gravity (mixed) 1.94 kg/L (ASTM C97)
زمن الجفاف 6 hours (ASTM-D1640)
Drying Time — Fully Cured 7 days
Technical Information — Compressive Strength 17.8 N/mm² (ASTM C170)
Technical Information — Compressive Test* Load 47400 N (ASTM C170)
Technical Information — Flexural Test* Load 925 N (ASTM C120) Flexural strength : 9.7 N/mm² (ASTM C120) *When mixing components A and B with 16 kg of filler (diameter: 3 to 6 mm)